1, phenomenon: Because the binding energy force of paint and card is abate,can appear lacquer phenomenon. Slowly paint surface can appear like scale account other people drop, drop with respect to what can present a state in brim region at the surface. This kind of phenomenon can in time discover, suffer from us to be able to in time undertake handling with never to be seen again.
2, reason: Got possibly in the process that sail or maintains all right agent of ketone of candle, grease, silicon, oily, drawing of patterns, water, ferruginous or of the material such as suds erode. Before be being used when did not undertake handling through metallic finishing agent, the model that perhaps uses paint is incorrect and brought about adhesion of tool reference plane insufficient.
In the process of spray paint temperature was not controlled good, the method is impertinent make its paint did not get sufficient dry. The viscosity that paints in the course that chooses paint is impertinent, model quality is not quits reduce airy pressure exorbitant. The stress that did not eliminate face of photograph adjacent lacquer to appear makes heavy panel of its lacquer face.
3, the method of processing: It is to clean plate tool reference plane seriously above all, accomplish dry, clean; Next right use finishing dose undertakes handling, spray paint is undertaking after awaiting period of time. The burnish before spray paint is very important also, also should accomplish dry, clean; Finally, want to make its paint successive job is having after complete solidify in the process with dry spray paint.
4, proposal: Do not want optional spray, the garage that seeks major undertakes spray paint. The masters that also can seek advice from major encounter such thing how should be we handled, do not make fun of petty trick to should change plate is decisive change, lest get legal punish.